高性能Sm2Co17型烧结永磁体的制备及微结构研究Preparation and Microstructures of Sm2Co17-type Sintered Magnets with High Magnetic Properties
王帅,雍辉,侯卫宵,马江微,崔燕,王志成
摘要(Abstract):
高性能2∶17型SmCo永磁体的磁性能和其微结构密切相关。通过优化Cu含量以及微结构制备出最大磁能积((BH)_(max))为32.88MGOe的高性能SmCo永磁体,并且磁体具有较高内禀矫顽力(H_(cj)).研究了磁体内禀矫顽力和微结构的关联。研究表明,随着Cu含量增加,磁体剩磁B_r逐渐减小,H_(cj)逐渐增大。Cu含量对Sm(Co_(bal)Cu_xFe_(0.285)Zr_(0.023))_(7.6)(x=0.051、0.062、0.073)磁体胞尺寸和片状相密度几乎没有影响,但随着Cu含量由0.051增加到0.073,胞壁处峰值Cu浓度明显增大,这是磁体内禀矫顽力增强的主要原因。
关键词(KeyWords): Sm_2Co_(17)型烧结永磁体;Cu含量;微观结构;磁性能
基金项目(Foundation): 太原科技大学博士科研启动基金(20202041)
作者(Author): 王帅,雍辉,侯卫宵,马江微,崔燕,王志成
参考文献(References):
- [1] 胡伯平,饶晓雷,王亦忠.稀土永磁材料[M].北京:冶金工业出版社,2017.
- [2] LIU J F,CHUI T,DIMITROV D,et al.Abnormal temperature dependence of intrinsic coercivity in Sm(Co,Fe,Cu,Zr)z powder materials[J].Applied Physics Letters,1998,73(20):3007-3009.
- [3] GUTFLEISCH O,WILLARD M A,BRüCK E,et al.Magnetic materials and devices for the 21st century:stronger,lighter,and more energy efficient[J].Advanced Materials,2011,23(7):821-842.
- [4] JIANG C B,AN S Z.Recent progress in high temperature permanent magnetic materials[J].Rare Metals,2013,32:431-440.
- [5] COEY J M D.Perspective and prospects for rare earth permanent magnets[J].Engineering,2020,6:119-131.
- [6] TRENCH A,SYKES J P.Rare earth permanent magnets and their place in the future economy[J].Engineering,2020,6:115-118.
- [7] LIU S,RAY A E.Sm2(Co,Fe,Cu,Zr)17 magnets with higher Fe content[J].IEEE Transactions on Magnetics,1989,25(5):3785-3787.
- [8] RAY A E.Metallurgical behavior of Sm(Co,Fe,Cu,Zr)z alloys[J].Journal of Applied Physics,1984,55(6):2094-2096.
- [9] TANG W,ZHANG Y,HADJIPANAYIS G C.Microstructure and magnetic properties of Sm(CobalFexCu0.128Zr0.02)7.0 magnets with Fe substitution[J].Journal of Magnetism and Magnetic Materials,2000,221:268-272.
- [10] WANG Y Q,SHANG Z F,YUE M,et al.Correlation between Fe content and z value in Sm(CobalFexCu0.06Zr0.025)z permanent magnets[J].Journal of Magnetism and Magnetic Materials,2019,474(15):417-423.
- [11] 朱明刚,孙威,方以坤,等.Sm2Co17基永磁材料的研究进展[J].中国材料进展,2015,34(11):789-795.
- [12] 王倩,王燕波,李扬,等.Cu含量对2∶17型SmCo永磁体磁畴结构和矫顽力的影响[J].稀有金属,2013,37(6):896-901.
- [13] 钟文定.铁磁学[M].北京:科学出版社,1998.
- [14] FENG H B,CHEN H S,GUO Z H,et al.Investigation on microstructure and magnetic properties of Sm2Co17 magnets aged at high temperature[J].Journal of Applied Physics,2011,109(7):07A763.
- [15] 田悦,夏卫星,徐晖,等.2∶17型烧结SmCo磁体磁畴壁钉扎机制[J].材料导报,2016,20:30-33.
- [16] ZHANG Y,CORTE-REAL M,HADJIPANAYIS G C,et al.Magnetic hardening studies in sintered Sm(Co,Cux,Fe,Zr)z 2∶17 high temperature magnets[J].Journal of Applied Physics,2000,87(9):6722-6724.
- [17] GOPALAN R,HONO K,YAN A,et al.Direct evidence for Cu concentration variation and its correlation to coercivity in Sm(Co0.74Fe0.1Cu0.12Zr.04)7.4 ribbons[J].Scripta Materialia,2009,60:764-767.
- [18] GOLL D,STADELMAIER H H,KRONMULLER H,et al.Samarium-cobalt 2∶17 magnets:Analysis of the coercive field of Sm2(CoFeCuZr)17 high-temperature permanent magnets[J].Scripta Materialia,2010,63:243-245.
- [19] LECTARD E,ALLIBERT C H,BALLOU R.Saturation magnetization and anisotropy fields in the Sm(Co1-xCux)5 phases[J].Journal of Applied Physics,1994,75(10):6277-6279.
- [20] SEPEHRI-AMIN H,THIELSCH J,FISCHBACHER J,et al.Correlation of microchemistry of cell boundary phase and interface structure to the coercivity of Sm(Co0.784Fe0.100Cu0.088Zr0.028)7.19 sintered magnets[J].Acta Materialia,2017,126:1-10.